 formula:

1. Self-use: use a small amount of asphalt to clean the emulsifier and mix it with water.

2. Thickening formula: asphalt cleaning emulsifier + super emulsifier + preservative + water + soluble acid and alkali resistant transparent thickening powder + wire-drawing powder + essence = asphalt cleaningagent

3. Non-consistency formula: asphalt cleaning emulsifier + super emulsifier + preservative + water + wire-drawing powder + essence = asphalt cleaning agent

2) proportion

1. (asphalt cleaning emulsifier + super emulsifier) 1-10%.

2. Wire drawing powder: add 100g to 200g per 100kg product.

3. Appropriate amount of preservative and essence. If you use it yourself, you can use it without preservative.

4. The quick-soluble acid-base transparent thickening powder should be 0.6-1%, depending on the required consistency.

2. Production process

Add the bituminous cleaning emulsifier, super emulsifier, wire-drawing powder, preservative and essence into the water and stir to dissolve

. It is necessary to add the instant acid - alkali - resistant transparent thickening powder after consistency.